Fabrication and analysis of deep submicron strained-Si n-MOSFET's

TL;DR: In this paper, deep submicron strained-Si n-MOSFETs were fabricated on strained Si/relaxed Si/sub 0.8/Ge/sub sub 0.2/ heterostructures to yield well matched channel doping profiles after processing, allowing comparison of strained and unstrained Si surface channel devices.
Abstract: Deep submicron strained-Si n-MOSFETs were fabricated on strained Si/relaxed Si/sub 0.8/Ge/sub 0.2/ heterostructures. Epitaxial layer structures were designed to yield well-matched channel doping profiles after processing, allowing comparison of strained and unstrained Si surface channel devices. In spite of the high substrate doping and high vertical fields, the MOSFET mobility of the strained-Si devices is enhanced by 75% compared to that of the unstrained-Si control devices and the state-of-the-art universal MOSFET mobility. Although the strained and unstrained-Si MOSFETs exhibit very similar short-channel effects, the intrinsic transconductance of the strained Si devices is enhanced by roughly 60% for the entire channel length range investigated (1 to 0.1 /spl mu/m) when self-heating is reduced by an ac measurement technique. Comparison of the measured transconductance to hydrodynamic device simulations indicates that in addition to the increased low-field mobility, improved high-field transport in strained Si is necessary to explain the observed performance improvement. Reduced carrier-phonon scattering for electrons with average energies less than a few hundred meV accounts for the enhanced high-field electron transport in strained Si. Since strained Si provides device performance enhancements through changes in material properties rather than changes in device geometry and doping, strained Si is a promising candidate for improving the performance of Si CMOS technology without compromising the control of short channel effects.

Content maybe subject to copyright    Report

Citations
More filters
Journal ArticleDOI
TL;DR: In this paper, the Si interstitials at the Si/oxide interface were injected into the underneath Si-SiGe heterojunction, and enhanced the Ge outdiffusion into the Si-oxide interface.
Abstract: The flicker noise characteristics of strained-Si nMOSFETs are significantly dependent on the gate oxide formation. At high temperature (900/spl deg/C) thermal oxidation, the Si interstitials at the Si/oxide interface were injected into the underneath Si-SiGe heterojunction, and enhanced the Ge outdiffusion into the Si/oxide interface. The Ge atoms at Si/oxide interface act as trap centers, and the strained-Si nMOSFET with thermal gate oxide yields a much larger flicker noise than the control Si device. The Ge outdiffusion is suppressed for the device with the low temperature (700/spl deg/C) tetraethylorthosilicate gate oxide. The capacitance-voltage measurements of the strained-Si devices with thermal oxide also show that the Si/oxide interface trap density increases and the Si-SiGe heterojunction is smeared out due to the Ge outdiffusion.

65 citations


Cites methods from "Fabrication and analysis of deep su..."

  • ...mobility enhancement obtained by low temperature process has been reported previously [9]....

    [...]

Journal ArticleDOI
TL;DR: In this article, the dependence of electron inversion layer mobility on high-channel doping required for sub-50-nm MOSFETs in strained silicon (Si), and compare it to co-processed unstrained Si.
Abstract: In this letter, we investigate the dependence of electron inversion layer mobility on high-channel doping required for sub-50-nm MOSFETs in strained silicon (Si), and we compare it to co-processed unstrained Si. For high vertical effective electric field E/sub eff/, the electron mobility in strained Si displays universal behavior and shows enhancement of 1.5-1.7/spl times/ compared to unstrained Si. For low E/sub eff/, the mobility for strained Si devices decreases toward the unstrained Si data due to Coulomb scattering by channel dopants.

64 citations


Cites background from "Fabrication and analysis of deep su..."

  • ...One promising candidate is strained Si where mobility enhancements in the 1.7‐2X range have been reported in relatively lightly doped channels [ 3 ], [4], motivating this study of dependence of electron mobility on channel doping....

    [...]

Journal ArticleDOI
TL;DR: In this paper, the performance enhancement degrades linearly as the gate length becomes shorter, due to not only the parasitic resistance but also heavy halo implant, thus the key integration issues are how to manage threshold difference and As diffusion without excess doping.
Abstract: Strained-Si nMOSFETs with a standard polysilicon gate process were fabricated down to 25 nm gate length with well-behaved characteristics and small difference in short channel effects. The performance enhancement degrades linearly as the gate length becomes shorter, due to not only the parasitic resistance but also heavy halo implant. Thus the key integration issues are how to manage threshold difference and As diffusion without excess doping. With comparable doping and well controlled parasitic resistance, up to 45% improvement in drive current is predicted for sub-50 nm gate length strained-Si nMOSFETs on the Si/sub 0.8/Ge/sub 0.2/ substrate. In this work approximately 45% enhancement is in fact demonstrated for 35 nm gate length devices, through advanced channel engineering and implementation of metal gates.

64 citations

Patent
09 Feb 2004
TL;DR: The planarization before the device epitaxial layers are deposited ensures a flat surface for state-of-the-art lithography as mentioned in this paper, allowing the MOSFET channel to be either at the surface or buried, one can create high speed digital and/or analog circuits.
Abstract: Structures and methods for fabricating high speed digital, analog, and combined digital/analog systems using planarized relaxed SiGe as the materials platform. The relaxed SiGe allows for a plethora of strained Si layers that possess enhanced electronic properties. By allowing the MOSFET channel to be either at the surface or buried, one can create high-speed digital and/or analog circuits. The planarization before the device epitaxial layers are deposited ensures a flat surface for state-of-the-art lithography.

61 citations

Journal ArticleDOI
TL;DR: In this article, the authors investigated elastic strain relaxation of free-standing SiGe/Si structures without the introduction of dislocations or other defects, and reported strained Si layers with biaxial tensile strain equal to 0.007 and 0.012.
Abstract: We have investigated elastic strain relaxation, i.e., strain relaxation without the introduction of dislocations or other defects, in free-standing SiGe/Si structures. We fabricated free-standing Si layers supported at a single point by an SiO2 pedestal and subsequently grew an epitaxial SiGe layer. The measured strain relaxation of the SiGe layer agrees well with that calculated using a force-balance model for strain sharing between the SiGe and strained Si layers. We report strained Si layers with biaxial tensile strain equal to 0.007 and 0.012.

59 citations

References
More filters
Journal ArticleDOI
TL;DR: In this article, the authors compute the band structure and shear deformation potentials of strained Si, Ge, and SiGe alloys, and fit the theoretical results to experimental data on the phonon-limited carrier mobilities in bulk Si and Ge.
Abstract: Using nonlocal empirical pseudopotentials, we compute the band structure and shear deformation potentials of strained Si, Ge, and SiGe alloys. Fitting the theoretical results to experimental data on the phonon‐limited carrier mobilities in bulk Si and Ge, the dilatation deformation potential Ξd is found to be 1.1 eV for the Si Δ minima, −4.4 eV for the Ge L minima, corresponding to a value for the valence band dilatation deformation potential a of approximately 2 eV for both Si and Ge. The optical deformation potential d0 is found to be 41.45 and 41.75 eV for Si and Ge, respectively. Carrier mobilities in strained Si and Ge are then evaluated. The results show a large enhancement of the hole mobility for both tensile and compressive strain along the [001] direction, but only a modest enhancement (approximately 60%) of the electron mobility for tensile biaxial strain in Si. Finally, from a fit to carrier mobilities in relaxed SiGe alloys, the effective alloy scattering potential is determined to be about 0...

1,500 citations

Journal ArticleDOI
TL;DR: In this paper, the inversion layer mobility in n-and p-channel Si MOSFETs with a wide range of substrate impurity concentrations (10/sup 15/ to 10/sup 18/ cm/sup -3/) was examined.
Abstract: This paper reports the studies of the inversion layer mobility in n- and p-channel Si MOSFET's with a wide range of substrate impurity concentrations (10/sup 15/ to 10/sup 18/ cm/sup -3/). The validity and limitations of the universal relationship between the inversion layer mobility and the effective normal field (E/sub eff/) are examined. It is found that the universality of both the electron and hole mobilities does hold up to 10/sup 18/ cm/sup -3/. The E/sub eff/ dependences of the universal curves are observed to differ between electrons and holes, particularly at lower temperatures. This result means a different influence of surface roughness scattering on the electron and hole transports. On substrates with higher impurity concentrations, the electron and hole mobilities significantly deviate from the universal curves at lower surface carrier concentrations because of Coulomb scattering by the substrate impurity. Also, the deviation caused by the charged centers at the Si/SiO/sub 2/ interface is observed in the mobility of MOSFET's degraded by Fowler-Nordheim electron injection. >

1,389 citations

Journal ArticleDOI
TL;DR: In this paper, the thermal resistivity, Seebeck coefficient, electrical resistivity and Hall mobility of GeSi alloys have been measured throughout the GeSi alloy system as functions of impurity concentration in the range 2×1018−4×1020cm−3, and of temperature in range 300°-1300°K.
Abstract: The thermal resistivity, Seebeck coefficient, electrical resistivity, and Hall mobility of Ge‐Si alloys have been measured throughout the Ge‐Si alloy system as functions of impurity concentration in the range 2×1018−4×1020cm−3, and of temperature in the range 300°–1300°K. A qualitative interpretation of these properties is given. For power conversion, boron and phosphorus were found to be useful p‐type and n‐type impurities, respectively, because of their high solid solubilities. At 1200°K, the maximum values of the dimensionless figure of merit zT were 0.8 for p‐type Ge0.15‐Si0.85 alloy doped to 2.1×1020cm−3 holes, and 1.0 for n‐type Ge0.15‐Si0.85 alloy doped to 2.7×1020cm−3 electrons. The maximum over‐all efficiency of a stable generator operating between 300°–1200°K, using the best p‐type and n‐type materials was computed to be 10%.

556 citations

Journal ArticleDOI
TL;DR: In this paper, the authors investigated the phonon-limited mobility of strained Si metal-oxide-semiconductor field effect transistors (MOSFETs) through theoretical calculations including two-dimensional quantization.
Abstract: The phonon‐limited mobility of strained Si metal–oxide–semiconductor field‐effect transistors (MOSFETs) fabricated on a SiGe substrate is investigated through theoretical calculations including two‐dimensional quantization, and compared with the mobility of conventional (unstrained) Si MOSFETs. In order to match both the mobility of unstrained Si MOSFETs and the mobility enhancement in strained Si MOSFETs, it is necessary to increase the coupling of electrons in the two‐dimensional gas with intervalley phonons, compared to the values used in conventional models. The mobility enhancement associated with strain in Si is attributed to the following two factors: the suppression of intervalley phonon scattering due to the strain‐induced band splitting, and the decrease in the occupancy of the fourfold valleys which exhibit a lower mobility due to the stronger interaction with intervalley phonons. While the decrease in the averaged conductivity mass, caused by the decrease in the occupancy of the fourfold valle...

454 citations

Journal ArticleDOI
TL;DR: In this paper, the authors developed a technique for measuring the thermal conductivity of silicon-on-insulator (SOI) transistors and provided data for layers in wafers fabricated using bond-and-etch-back (BESOI) technology.
Abstract: Self heating diminishes the reliability of silicon-on-insulator (SOI) transistors, particularly those that must withstand electrostatic discharge (ESD) pulses. This problem is alleviated by lateral thermal conduction in the silicon device layer, whose thermal conductivity is not known. The present work develops a technique for measuring this property, and provides data for layers in wafers fabricated using bond-and-etch-back (BESOI) technology. The room-temperature thermal conductivity data decrease with decreasing layer thickness, d s , to a value nearly 40 percent less than that of bulk silicon for d s = 0.42 μm, The agreement of the data with the predictions of phonon transport analysis between 20 and 300 K strongly indicates that phonon scattering on layer boundaries is responsible for a large part of the reduction. The reduction is also due in part to concentrations of imperfections larger than those in bulk samples. The data show that the buried oxide in BESOI wafers has a thermal conductivity that is nearly equal to that of bulk fused quartz. The present work will lead to more accurate thermal simulations of SOI transistors and cantilever MEMS structures.

358 citations