How do you remove corrosion from a water valve? 

Answers from top 9 papers

More filters
Papers (9)Insight
The products of corrosion enter the water, diminishing its quality, and may become a health hazard.
These results indicate that water adsorption is crucial for initializing atmospheric corrosion.
The results indicate that flow control valve body failed due to combination of hydrogen induced corrosion cracking (HICC) and sulfide stress corrosion cracking (SSCC).
A novel corrosion indicator, “corrosion inhibitory effect of cations Y”, that consists of X and molar volume ratio, ΔV, is proposed, and it is shown that the novel indicator can estimate the corrosion rate of mild steel in fresh water.
It is found that a higher flow rate induces a higher corrosion rate in various water containing conditions, which becomes much obvious with increasing the water concentration.
The results show that this environmental friendly corrosion inhibitor at relatively low dosages had a good inhibition effect on the carbon steel corrosion in soft water.
Journal ArticleDOI
Gonzalo Pizarro, Ignacio T. Vargas 
01 Aug 2016-Water supply
11 Citations
The results of this work highlight the necessity to incorporate the hydrodynamic effects in the analysis of corrosion and corrosion by-products release into drinking water piping systems.
Considering the corrosion of the whole steam–water system, a more effective feedwater chemistry treatment method is proposed.
Concurrently, the thermodynamic calculation suggests that impurities change the corrosion process through promoting the water precipitation and changing the water chemistry characteristics.

See what other people are reading

How does quenching and tempering affect the mechanical properties of deformation tube anchors?
5 answers
Quenching and tempering processes significantly influence the mechanical properties of deformation tube anchors. The quenching and tempering treatments lead to a change in the microstructure of the steel, affecting its strength, toughness, and impact energy. Different tempering temperatures result in varying mechanical properties, with higher temperatures generally leading to decreased strength but increased impact toughness. The stabilization mechanism of residual austenite in high-alloyed steel also plays a crucial role in determining the mechanical properties after such treatments. Additionally, the new quenching and tempering process proposed for steel tubes enhances properties like high strength, wear-resistance, plasticity, and pressure-resistance, meeting the technological requirements for hydraulic cylinder casings. Overall, these processes optimize the material's properties for deformation tube anchors.
What are the current advancements in the production and utilization of Fourth-Generation Biodiesel?
4 answers
Current advancements in Fourth-Generation Biodiesel production and utilization include genetic and metabolic engineering tools enhancing the production of long-chain hydrocarbons, bioethanol, and fatty acids from microalgae. Additionally, the synthesis of magnetic catalysts has shown promise in improving biodiesel production, with various types such as mixed metal oxides, supported catalysts, and metal-organic framework-based catalysts being explored for their physicochemical properties and reusability. Furthermore, the use of advanced technologies like enzymatic or heterogeneous catalysts in supercritical environments offers cost-effective and sustainable alternatives to traditional homogeneous catalytic transesterification processes, allowing for easier separation of biodiesel from reaction mixtures and catalyst recovery. These advancements pave the way for a more efficient and environmentally friendly production and utilization of Fourth-Generation Biodiesel as a sustainable alternative energy source.
How does the use of piezoelectric materials affect waterproofing in electronic devices?
5 answers
The use of piezoelectric materials in electronic devices impacts waterproofing by necessitating specialized coatings and sealing methods to enhance reliability and longevity. Piezoelectric flexible microdevices for marine applications require waterproofing to prevent water absorption, corrosion, and biofilm formation. Incorporating piezoelectric elements in devices like ultrasonic transducers demands multiple sealing mechanisms to achieve complete waterproofing, even under high water pressure. Methods such as coating with silane and injecting fluoride to form a continuous waterproofing membrane have been proposed to isolate the main board from water ingress, improving waterproof reliability. Additionally, applying a paint of constant thickness on housing joints can simplify waterproofing processes in electronic devices. These strategies highlight the importance of tailored waterproofing solutions when utilizing piezoelectric materials in electronic devices.
How does titanium dioxide contribute to the waterproofing properties of these sprays?
5 answers
Titanium dioxide (TiO2) plays a crucial role in enhancing the waterproofing properties of various sprays. TiO2 anisotropic nanocrystal rods (TiO2 NRs) dispersed in n-heptane demonstrated superior dispersibility and processability, making it the optimal solvent for TiO2 NR dispersion. Coatings with mesoporous TiO2 exhibited the best corrosion performance due to strong interactions with the polymeric matrix, resulting in high barrier properties. TiO2-coated clay roofing tiles showed superhydrophilic properties, enhancing water contact angle measurements and promoting self-cleaning effects. Additionally, TiO2 nanoparticles in conjunction with metallic nanoparticles improved the biocidal efficiency of coatings on porous limestone, maintaining high photocatalytic and self-cleaning efficiencies even after prolonged exposure to UV light and stains.
What are the specific environmental benefits of using eco-composites in engineering applications?
5 answers
The utilization of eco-composites in engineering applications offers significant environmental benefits. These composites, such as those reinforced with recycled polyethylene waste and natural fibers, help reduce industrial waste and pollution. By incorporating materials like polyethylene and natural fibers into composites, the environmental impact of traditional materials like cement and metal is lessened. Eco-composites exhibit excellent mechanical properties, making them suitable for various engineering applications while promoting sustainability and ecosystem conservation. Furthermore, the development of eco-friendly composites contributes to the preservation of natural resources, reduction of water pollution, and prevention of material corrosion. Overall, the use of eco-composites in engineering not only enhances performance but also aligns with the global goal of sustainable and environmentally friendly practices.
How does Fe2 become Fe3 when sulfide nano zero valent iron degrades organics?
5 answers
The transformation of Fe^2+ to Fe^3+ during the degradation of organics by sulfide nano zero-valent iron (S-nZVI) is a multifaceted process that involves various mechanisms, as elucidated by the research contexts provided. The core principle behind this transformation lies in the reactivity and interaction of S-nZVI with organic pollutants and the subsequent generation of reactive oxygen species (ROS) and other oxidative species. In the degradation process, S-nZVI exhibits high reactivity towards halogenated organic pollutants, where the sulfurization of nZVI enhances both its stability and activity, leading to effective pollutant degradation. The sulfurization process, as described, involves the formation of a core-shell structure or a mixture of FeS2 and nZVI, which significantly contributes to the degradation efficiency. The biological precipitation method developed for preparing S-nZVI, which avoids harmful chemical sulfidating agents, also plays a crucial role in enhancing the reactivity and selectivity of S-nZVI towards pollutants. The activation of strong oxidants like persulfate (PS) by nano-Fe^0, which is a component of S-nZVI, generates sulfate radicals (SRs) that possess higher oxidation potentials. This process is instrumental in the degradation of refractory organics, where Fe^0 acts as a catalyst. Similarly, the activation of peroxymonosulfate (PMS) and peroxydisulfate (PDS) by activated zero-valent iron (Ac-ZVI) coupled with Fe^3+ leads to the liberation of Fe^2+ as an active species for ROS generation, further facilitating organic degradation. The transformation from Fe^2+ to Fe^3+ occurs as part of the oxidative processes involved in the degradation of organics. The presence of Fe^3+ promotes the liberation of Fe^2+ from Ac-ZVI, which then participates in the generation of ROS. These ROS, including sulfate radicals, are responsible for the oxidative degradation of pollutants. As Fe^2+ is oxidized during these reactions, it is converted into Fe^3+, which can then be recycled back into the system to promote further Fe^2+ liberation and ROS generation, thus sustaining the degradation process. Moreover, the modification of nZVI with sulfur and other agents, as discussed across various contexts, not only improves the dispersity and stability of nZVI in aqueous solutions but also enhances its reactivity towards organic pollutants by facilitating the generation of oxidative species and the transformation of Fe^2+ to Fe^3+ during the degradation process. This transformation is crucial for the continuous and effective degradation of organics, making S-nZVI a potent material for the remediation of contaminated water and soil.
Is rutin lipophilic and soluble in plant oils?
5 answers
Yes, rutin can be made lipophilic through esterification with fatty acids like oleic acid, enhancing its solubility in oils. Studies have successfully synthesized lipophilic rutin derivatives, such as rutin oleate and decaacetylated rutin, which showed improved solubility and permeability. Rutin's solubility has been explored in supercritical carbon dioxide and subcritical 1,1,1,2-tetrafluoroethane, indicating its potential for extraction from plant tissues. Additionally, the development of rutin phytosomes has shown increased aqueous solubility and enhanced transdermal permeation, making it suitable for topical applications in inflammatory conditions. Therefore, rutin can be modified to be lipophilic and soluble in plant oils through various chemical modifications, offering versatility for different applications.
How do nanobubbles impact heating and cooling water systems?
5 answers
Nanobubbles play a crucial role in heating and cooling water systems by influencing scale inhibition, corrosion inhibition, and heat transfer enhancement. In circulating cooling water systems, air nanobubbles (A-NBs) exhibit a high scale inhibition rate due to their ability to adsorb cations, microcrystals, and form a bubble layer, preventing scale deposition. Additionally, A-NBs have shown significant corrosion inhibition effects on brass surfaces by promoting passivation film formation and bubble layer development. Nanofluids containing nanoparticles like alumina have been found to enhance heat transfer in pool boiling systems, leading to reduced surface temperatures and increased heat transfer coefficients. Furthermore, nanobubbles have been utilized to alter material properties, affecting density, fluidity, and temperature variations in aqueous solutions. Overall, nanobubbles positively impact heating and cooling water systems through scale and corrosion inhibition as well as heat transfer enhancement.
What is Type IV Cracks in weld joint/?
5 answers
Type IV cracks in weld joints refer to a specific type of failure mechanism observed in high-chromium ferritic steels like P91 and P22 used in high-temperature applications. These cracks typically initiate in the fine-grained heat-affected zone (FGHAZ) or intercritical HAZ due to microstructure gradients, leading to strain localization and eventual crack formation. Type IV cracks are associated with creep failures, where creep cavity accumulation and thermal displacement contribute to stress concentration and crack development. Non-destructive evaluation methods struggle to detect dense creep voids before crack initiation, making early detection challenging. Research focuses on understanding the micromechanical and microstructural origins of Type IV failures, highlighting factors like grain boundary sliding, grain boundary cavities, and diffusion-controlled creep fracture mechanisms. These insights aid in predicting and preventing premature failures in welded components operating at elevated temperatures.
What methods are commonly used to plot response spectrum vs time period for seismic data analysis?
5 answers
The methods commonly used to plot response spectrum versus time period for seismic data analysis include the Independent Support Motion (ISM) method, Spectrum Method Assisted by Time History Analysis (SATH) method, inelastic response spectrum method, and time-domain iteration methods. The ISM approach may lead to overestimation in group responses under certain rules, prompting the development of the SATH method for more realistic results. Additionally, a simplified method utilizing inelastic response spectrum has been developed to consider uncertainties in time history analysis, offering a practical alternative to time-consuming nonlinear analyses. Furthermore, time-domain nonlinear methods like the dynamic skeleton curve constitutive model and expanded Masing criterion are effective in capturing the nonlinear behavior of soft soil layers in seismic response analysis.
What are de advantages and desavantages of the igneus rocks in civil engineering?
5 answers
Igneous rocks offer several advantages and disadvantages in civil engineering. In terms of advantages, fine-grained and basic igneous rocks exhibit higher engineering quality and lower abrasiveness potential compared to acidic and coarse-grained ones. Additionally, the incorporation of pumice powder in traditional cementitious materials can enhance properties such as thermal and acoustic insulation, fire resistance, and resistance to various chemical agents. On the other hand, some disadvantages include the negative impact of porosity on the dry density of rock samples and the decrease in modulus of elasticity with increasing temperature in igneous rocks. Moreover, the use of igneous glass powder in concrete can improve anti-seepage, anti-corrosion, durability, and environmental protection properties, although it may negatively affect workability and mechanical strength.