TL;DR: In this article, the enthalpy relaxation behavior of poly(l-lactide) (PLLA) below glass transition temperature (Tg) and its effects on the mechanical properties were studied using differential scanning calorimetry (DSC), dynamic mechanical thermal analysis (DMTA), and tensile test.
Abstract: The enthalpy relaxation behavior of poly(l-lactide) (PLLA) below glass transition temperature (Tg) and its effects on the mechanical properties were studied using differential scanning calorimetry (DSC), dynamic mechanical thermal analysis (DMTA), and tensile test. Both the enthalpy loss (δH) and peak endothermic temperature (Tp) in the glass transition region show a linear increase with the logarithm of aging time (ta). On the basis of DSC results, the kinetics of the enthalpy relaxation process were analyzed, and the kinetic parameters of PLLA were obtained: relaxation rate of enthalpy at 40 °C βH = 1.77 J g-1 per decade, and apparent activation energy Δh* = 1107 kJ mol-1. Besides, analysis on the kinetic of enthalpy relaxation for poly(dl-lactide) (PDLLA) shows that the Δh* value of PDLLA is similar to that of PLLA. Moreover, it was found that the strength and modulus of PLLA increase gradually; on the contrary, the toughness reduces dramatically during the physical aging. The yield strength and tensi...
223 citations
••
TL;DR: The results show that the better disperse morphology of HA grains using the experiment methods, and PDLLA/HA composites at a definite range of compound ratio have much better shape memory effect than pure PD LLA polymer.
223 citations
••
TL;DR: A Ni-Ti alloy, generically called nitinol, was prepared from sputtering targets of two different compositions on glass substrates using a dc magnetron source, and the as-deposited films were amorphous in structure and did not exhibit a shape memory as mentioned in this paper.
Abstract: A Ni-Ti alloy, generically called nitinol, was prepared from sputtering targets of two different compositions on glass substrates using a dc magnetron source. The as-deposited films were amorphous in structure and did not exhibit a shape memory. The amorphous films were crystallized with a suitable annealing process, and the transformation properties were measured using differential scanning calorimetry. The annealed films demonstrated a strong shape-memory effect. Stress/strain measurements and physical manipulation were used to evaluate the shape recovery. These tests demonstrated sustained tensile stresses of up to 480 MPa in the high-temperature phase, and a characteristic plastic deformation in the low-temperature phase.
223 citations
••
TL;DR: In this article, a comparative study was conducted to determine the oxidative stability of twelve different edible oils with two different instruments: a differential scanning calorimeter and an oxidative stability index (OSI) instrument.
222 citations
••
TL;DR: The phase transition temperature and values of latent heat of eutectic mixtures of CA and LA are suitable for being incorporated with building materials to form phase change wallboards used for building energy storage.
222 citations