Method for preparing high-pruity alumina powder

Reads0
Chats0
TLDR
In this paper, a method to produce highly pure Alumina powder is described. The steps are as follows: deploying Aluminium hydroxide which is produced in the process of manufacturing alumina using sintering process to be solution, disposing of impurity, adding seed crystal to prepare highly pure aluminium hydroxides; removing Na in the solution, getting highly pure bodhmite after hydrothermal synthesis; and after washing and baking, highly pure Albina can be obtained.
Abstract
The invention discloses a method to produce highly pure Alumina powder. The steps are as follows: deploying Aluminium hydroxide which is produced in the process of manufacturing alumina using sintering process to be solution, disposing of impurity, adding seed crystal to prepare highly pure aluminium hydroxide; removing Na in the solution, getting highly pure bodhmite after hydrothermal synthesis; and after washing and baking, highly pure Alumina can be obtained. The cost is about 15 thousand per ton, which is far less than current market price, 40-60 thousand per ton. It can put into production in a large scale and it is easy to reach 1-5 thousand ton per year. With a low cost, no pollution and high purity (over 99.99 percent), the production is widely used in rare earth fluorescence materials, high voltage Na lamp and other relative special Alumina fine ceramics field.

read more

Citations
More filters
Patent

Method for reducing content of sodium in aluminum hydroxide

TL;DR: In this paper, a method for reducing the content of sodium in aluminum hydroxide was proposed, in particular for preparing low-sodium aluminum hydride (Na2O is less than 0.1 percent) serving as a fire retardant or a raw material for calcining lowsodium alpha-aluminum oxide.
Patent

Method for electrochemically preparing high-purity aluminum oxide

TL;DR: In this article, a method for electrochemically preparing high-purity aluminum oxide, which comprises the following steps of: taking an electrolytic aluminum ingot with a purity of 99 percent as an anode, graphite with pure spectrum as a cathode and alkaline liquor with a pH value of 8-10 as an electrolyte, switching on direct current, applying the voltage of 1.7-2.0 V for electrolysis and controlling the electrolysis temperature within 18-45 DEG C.
Patent

Preparation technology of highly pure alumina powder

TL;DR: In this paper, a two-stage solution purification on a raw material industrial sodium aluminate solution was described, in which a crystal seed initiator and a sodium precipitation inhibitor were added to the pure sodium alumina solution to prepare a seed slurry, and then a high temperature calcining on the pure aluminum hydroxide, water quenching, and washing was performed to obtain the highly pure alumina powder.
Patent

Method for preparing high-purity superfine Alpha-Al2O3 powder from microemulsion

Jingjing Ma, +1 more
TL;DR: In this article, a method for preparing high-purity superfine Alpha-Al2O3 powder from a micro-emulsion is presented, which comprises the following steps of: selecting corresponding aqueous phase, oil phase, a surfactant and a cosurfactant according to the property of the microemulsion; preparing an aluminum chloride emulsion, uniformly stirring, adding ammonia water or ammonium bicarbonate to adjust pH to 8-10, hydrolyzing in a water bath for 20-90min at 50-100 DEG C, carrying out
Patent

Preparation method of submicron alumina

TL;DR: In this article, a preparation method of submicron alumina for a film coating layer is described, which is characterized in that the preparation process comprises the steps: (1) carrying out a reaction of aluminum hydroxide with sodium hydroxides to generate a sodium aluminate solution; (2) adopting a nitric acid solution added with a mineralizer, and carrying out neutralization titration reaction; (3)carrying out aging, suction filtration, washing and drying of a precipitation, and thus obtaining pseudo-boehmite; (4)