scispace - formally typeset
Patent

Middle-temperature acidic electroless nickel plating-phosphor alloy formula

Reads0
Chats0
TLDR
In this article, the authors provided a formulation of medium-temperature acidic electroless nickel-phosphorus alloy, which is characterized in that the formulation is as follows: 25 to 30 grams of nickel sulfate per liter, 25 to 35 grams of sodium hypophosphite per liter.
Abstract
The invention provides a formulation of medium-temperature acidic electroless nickel-phosphorus alloy, which is characterized in that the formulation is as follows: 25 to 30 grams of nickel sulfate per liter, 25 to 35 grams of sodium hypophosphite per liter, 12 to 18 grams of sodium acetate per liter, 05-13 milligrams of thiourea per liter, 7 to 13 milliliters of lactic acid per liter, 7 to 13 milliliters of acetic acid per liter, 4-10 grams of organic acid per liter, 5-16 milligrams of potassium iodide or potassium iodate per liter, and the loadage is between 05 and 15 dm /L The invention has the advantages that: the formulation improves the stability of a plating solution, obviously improves plating rate, has good corrosion resistance and the comprehensive properties of plating; the stability of the plating solution can reach over 1800 s; the stability of periodic experiments is more than ten periods; the corrosion resistance of the plating reaches over 130 s; and the hardness of the plating reaches 480 HV

read more

Citations
More filters
Patent

Phosphatizing liquid and preparation method thereof

Jing Yangfu
TL;DR: In this paper, the phosphatizing liquid comprises the following components in percentage by weight: 7 percent of starter liquid, 0.4 to 0.6 percent of accelerator and the balance of water.
Patent

High-phosphorus chemical nickel-plating concentrated solution and plating process

TL;DR: In this paper, a high-phosphorus chemical nickel-plating concentrated solution and a plating process is described, which is suitable for application in brazing, spot welding and depositing a thick coating.
Patent

Environment-friendly type high hydrogen sulfide resistant and high wear-resistant Ni-P-W-Mo quaternary alloy plating solution and its preparation method

Deng Chaoying, +1 more
TL;DR: In this article, a Ni-P-W-Mo quaternary alloy plating solution is described. But the plating solutions are not suitable for the use with heavy metal ion environmental pollution.
Patent

Chemical plating solution of oilfield drilling tool and anti-corrosion protection method of drilling tool

TL;DR: In this paper, a chemical plating solution of an oilfield drilling tool and an anti-corrosion protection method of the drilling tool are described. But the method is not suitable for the use in the real world.
Patent

Nickel-phosphorus/nano V8C7 composite plating liquid

TL;DR: The composite plating liquid is simple in composition, little in damage of reagents to the environment, stable in technology, simple in operation, and high in current efficiency as mentioned in this paper.