Composite magnetic core

TLDR
In this article, a magnetic core main body composed of flat-shaped soft magnetic alloy material and insulator and a metal outer pipe accommodating said core is provided, and the flat surface of the soft magnetic Alloy material is orientated in the axial direction of the outer pipe.
Abstract
PURPOSE: To reduce magnetic gap, and improve magnetic characteristics, by providing a magnetic core main body composed of flat-shaped soft magnetic alloy material and insulator and a metal outer pipe accommodating said core, orientating the flat surface of the soft magnetic alloy material in the axial direction of the material outer pipe, and substantially constituting the soft magnetic alloy material in an amorphous state. CONSTITUTION: Magnetic core main body composed of flat-shaped soft magnetic alloy material and insulator and a metal outer pipe accommodating said core are provided, and the flat surface of the soft magnetic alloy material is orientated in the axial direction of the outer pipe. The soft magnetic alloy material is amorphous alloy expressed by Fe 100-a-b M a Y b . M is at least one kind of element selected out of group IV a , group V b elements in periodic table, and Mn, Co and Cu. Y is at least one of Si, B, P and C. The notations (a) and (b) represent at%, and adjustment is performed so as to satisfy 0≤a≤8 and 10≤b≤30. COPYRIGHT: (C)1992,JPO&Japio

read more

Citations
More filters
Patent

Flat soft magnetic metal powder and composite magnetic material including the soft magnetic metal powder

TL;DR: In this article, a flat soft magnetic metal powder is provided that includes Ni in the range of 60 to 90 mass %, one or more kinds of Nb, V, and Ta in the total (0.05 to 19.95 mass % when Mo is added thereto).
Patent

Fe-Ni-Mo FLAKY METAL SOFT MAGNETIC POWDER AND MAGNETIC COMPOSITE MATERIAL CONTAINING SOFT MAGNETIC POWDER

TL;DR: In this paper, the authors measured the X-ray diffraction pattern of Fe-Ni-Mo flaky metal soft magnetic powder with an aspect ratio (average particle size/average thickness) of 5-500 and the peak intensity ratio I200/I111 is in the range from 0.43 to 10.
Patent

Dust core and magnetic element

TL;DR: In this paper, the authors proposed a dust core that has improved magnetic characteristics and heat radiation properties and can maintain corrosion resistance over a long period, and to provide a reliable magnetic element having the dust core.
Patent

Magnetic powder and production method thereof, magnetic core and production method thereof, coil component and motor

TL;DR: In this article, a magnetic powder is represented by general formula Fe a (Si b B c P d ) 100-a, and is produced with a gas atomization method.
Patent

Fe-Ni-Mo soft magnetic flaky powder and magnetic composite material containing soft magnetic powder

TL;DR: In this paper, the authors proposed a soft magnetic flaky powder with oxide layer wherein an oxide layer of a thickness of 50 to 1000 Å is formed on the surface of this soft magnetic material.
References
More filters
Patent

Production of oxide superconductor

TL;DR: In this paper, an oxide superconductor thin film having high critical current density is obtained by lowering the temperature of the oxide super-conductor at <=5 degC/minute cooling velocity.
Patent

Fluid pressure cylinder

TL;DR: In this article, the brake packings 15, 36 are formed by uniting cushion packings 16, 38, 39 and brake shoes 17, 30, 39 in a body.
Patent

Tension calculating method

TL;DR: In this paper, the authors propose to detect the tension acting on a rolling material between rolling mills with good accuracy and to eventually permit the tension control with high accuracy even with a rolling installation having no sensors for detecting rolling load by using only the rolling power to be outputted by the main motors of the rolling mills without using the rolling load.