Journal ArticleDOI
Microconstituent-Induced Pitting Corrosion in Aluminum Alloy 2024-T3
TLDR
In this article, free corrosion immersion experiments were conducted on a commercial airframe material, Al 2024-T3 (UNS A92024), in 0.5 M sodium chloride (NaCl) solution to investigate the role of microcon...Abstract:
Free corrosion immersion experiments were conducted on a commercial airframe material, Al 2024-T3 (UNS A92024), in 0.5 M sodium chloride (NaCl) solution to investigate the role of microcon...read more
Citations
More filters
Journal ArticleDOI
Sol–gel coatings on metals for corrosion protection
Duhua Wang,Gordon P. Bierwagen +1 more
TL;DR: In this article, a review of the recent developments and applications of sol-gel corrosion protection coatings on different metal substrates, such as steel, aluminum, copper, magnesium and their alloys, is presented.
Journal ArticleDOI
Corrosion of AA2024-T3 Part I: Localised corrosion of isolated IM particles
TL;DR: In this paper, the development of corrosion around isolated intermetallic particles was monitored using scanning electron microscopy with energy dispersive X-ray spectroscopy (EDXS).
Journal ArticleDOI
Formation of a cerium-based conversion coating on AA2024: relationship with the microstructure
TL;DR: In this article, the nucleation and growth of the cerium-based conversion coating on AA2024 was studied using complementary surface analysis techniques, as atomic force microscopy in the Kelvin probe mode (SKPFM), scanning electron microscopy (SEM) and energy dispersive spectroscopy (EDS).
Journal ArticleDOI
A transmission electron microscopy study of constituent-particle-induced corrosion in 7075-T6 and 2024-T3 aluminum alloys
TL;DR: In this article, thin foil specimens of 7075-T6 and 2024-T3 aluminum alloys were immersed in aerated 0.5M NaCl solution and then examined by transmission electron microscopy (TEM).
Journal ArticleDOI
Transition from pitting to fatigue crack growth—modeling of corrosion fatigue crack nucleation in a 2024-T3 aluminum alloy
TL;DR: The nucleation of fatigue cracks from corrosion pits was investigated by conducting fatigue experiments on open-hole specimens of a 2024-T3 aluminum alloy in 0.5 M NaCl solution at room temperature and different load frequencies from 0.1 to 20 Hz.
References
More filters
Book
Aluminum: Properties and Physical Metallurgy
TL;DR: Aluminum as mentioned in this paper is a collection of 53 recognized experts on aluminium and aluminium alloys Joint venture by world renowned authorities-the Aluminium Association Inc. and American Society for Metals.