Nickel-Based Superalloys for Advanced Turbine Engines: Chemistry, Microstructure and Properties
Tresa M. Pollock,Sammy Tin +1 more
Reads0
Chats0
TLDR
The chemical, physical, and mechanical characteristics of nickel-based superalloys are reviewed with emphasis on the use of this class of materials within turbine engines as mentioned in this paper, and the role of major and minor alloying additions in multicomponent commercial cast and wrought super-alloys is discussed.Abstract:
The chemical, physical, and mechanical characteristics of nickel-based superalloys are reviewed with emphasis on the use of this class of materials within turbine engines. The role of major and minor alloying additions in multicomponent commercial cast and wrought superalloys is discussed. Microstructural stability and phases observed during processing and in subsequent elevated-temperature service are summarized. Processing paths and recent advances in processing are addressed. Mechanical properties and deformation mechanisms are reviewed, including tensile properties, creep, fatigue, and cyclic crack growth. I. Introduction N ICKEL-BASED superalloys are an unusual class of metallic materials with an exceptional combination of hightemperature strength, toughness, and resistance to degradation in corrosive or oxidizing environments. These materials are widely used in aircraft and power-generation turbines, rocket engines, and other challenging environments, including nuclear power and chemical processing plants. Intensive alloy and process development activities during the past few decades have resulted in alloys that can tolerate average temperatures of 1050 ◦ C with occasional excursions (or local hot spots near airfoil tips) to temperatures as high as 1200 ◦ C, 1 which is approximately 90% of the melting point of the material. The underlying aspects of microstructure and composition that result in these exceptional properties are briefly reviewed here. Major classes of superalloys that are utilized in gas-turbine engines and the corresponding processes for their production are outlined along with characteristic mechanical and physical properties.read more
Citations
More filters
Journal ArticleDOI
Design and development of a high-performance Ni-based superalloy WSU 150 for additive manufacturing
TL;DR: In this paper, a new Ni-based superalloy has been developed by the application of the combinatorial alloy development technique coupled with CALPHAD based solidification modeling by effectively suppressing the precipitation kinetics.
Journal ArticleDOI
Characterization of the Microstructure Evolution and Microsegregation in a Ni-Based Superalloy under Super-High Thermal Gradient Directional Solidification
Yongjun Zhang,Jianguo Li +1 more
TL;DR: In this paper, the microstructure evolution and microsegregation behavior of alloying elements in a Ni-based superalloy at a series of growth rates under super-high thermal gradient directional solidification were quantitatively characterized.
Journal ArticleDOI
Tailoring the Properties of a Ni-Based Superalloy via Modification of the Forging Process: an ICME Approach to Fatigue Performance
TL;DR: In this paper, an integrated computational materials engineering (ICME) framework is adopted to tailor the fatigue performance of a Ni-based superalloy, RR1000, and a deformation mechanism map and process models for grain boundary engineering of RR1000 are used to identify the optimal thermo-mechanical processing parameters to realize these desirable microstructural features.
Journal ArticleDOI
Evolution of oxides and their microstructures at 800°C in a γ-γ’ stabilised Co-Ni-Al-Mo-Ta superalloy
TL;DR: The mechanism of high temperature oxidation of the new γ'-strengthened Co-30Ni-10Al-5Mo-2Ta (at%) alloy was reported in this article.
Journal ArticleDOI
Sigma and Random Grain Boundaries and Their Effect on the Corrosion of the Ni-Cr-Mo Alloy 22
TL;DR: In this paper, the Ni-Cr-Mo alloy C22 was studied in a simulated crevice corrosion environment (3 M NaCl + 1.5 M HCl at 75◦C).
References
More filters
Book
Dislocations in solids
TL;DR: In this article, Bertotti, Ferro, and Mazetti proposed a theory of dislocation drag in covalent crystals and formed a model of the formation and evolution of dislocations during irradiation.
Journal ArticleDOI
Creep resistance of CMSX-3 nickel base superalloy single crystals
Tresa M. Pollock,A.S. Argon +1 more
TL;DR: In this paper, the authors studied the effect of dislocation-free nickel base superalloy single crystals with high volume fractions of the γ′ phase on their deformation and found that the dislocation free precipitates are resistant to shearing by dislocations.
Journal ArticleDOI
The precipitation of topologically close-packed phases in rhenium-containing superalloys
Catherine M.F. Rae,Roger C. Reed +1 more
TL;DR: In this paper, the formation of topologically close-packed (TCP) phases due to the addition of solid solution strengtheners, such as rhenium, molybdenum and tungsten, has been studied.
Journal ArticleDOI
Dynamic recrystallization in nickel and nickel-iron alloys during high temperature deformation
M.J Luton,C.M. Sellars +1 more
TL;DR: In this paper, it is established from metallographic and flow stress observations that dynamic recrystallization occurs at strains greater than a critical value and results in a recrystized grain size which is determined entirely by the flow stress.
Journal ArticleDOI
Creep behaviour of Ni-base single-crystal superalloys with various γ' volume fraction
TL;DR: In this article, a third generation Ni-base single-crystal superalloy TMS-75 and its γ/γ " tie line alloys were designed to contain various volume fractions of γ, while the compositions of two individual phases were kept the same.