Comparison of Fracture Load of the Four Translucent Zirconia Crowns.

Reads0
Chats0
Abstract
Recently, translucent zirconia has become the most prevalent material used as a restorative material. This study aimed to compare the crown fracture load of the four most common different translucent zirconia brands available in the market at 1.5 mm thickness. Standardized tooth preparations for a full ceramic crown were designed digitally with software (AutoCAD) by placing a 1.0 mm chamfer margin and 1.5 mm occluso-cervical curvature for the crown sample manufacturing. Stylized crowns were chosen to control the thickness of the crown. The axial and occlusal thickness were standardized to 1.5 mm thickness except at the central pit, which was 1.3 mm thick. The STL file for the tooth dies was prepared using software (3Shape TRIOS® Patient Monitoring, Copenhagen, Denmark). The tooth dies were printed with a resin material (NextDent Model 2.0, Vertex-Dental B.V., Soesterberg, The Netherlands) using a 3D printing software (3D Sprint® Client Version 3.0.0.2494) from a 3D printer (NextDent™ 5100, Vertex-Dental B.V., Soesterberg, The Netherlands). The printing layer thickness was 50 µm. Then, a total of twenty-eight (N = 28) stylized crowns were milled out of AmannGirrbach (Amann Girrbach GmbH, Pforzheim, Germany) (n = 7), Cercon HT (Dentsply Sirona, Bensheim, Germany) (n = 7), Cercon XT (Dentsply Sirona, Bensheim, Germany) (n = 7), and Vita YZ XT (Zahnfabrik, Bad Sackingen, Germany) (n = 7). Following sintering the crowns, sandblasting was performed and they were bonded to the tooth dies with the resin cement (RelyX U-200, 3M ESPE, Seefeld, Germany) and permitted to self-cure under finger pressure for 6 min. The crowns were loaded on the occlusal surface in a universal testing machine (MTS Centurion) with a stainless-steel ball indenter (7 mm radius) with a loading rate of 1 mm/min to contact the stylized crowns on each of the four cusps until failure. A rubber sheet (1.5 mm thickness) was positioned between the crown and indenter, which helped with the load distribution. Statistical analysis was done using SPSS version 20 (IBM Company, Chicago, USA). The fracture loads were analyzed using Dunnett's T3 test, and the number of cracks was analyzed using the Mann-Whitney U test among the groups. The significant level was set at p value = 0.05. The mean fracture loads were 3086.54 ± 441.74 N, 4804.94 ± 70.12 N, 3317.76 ± 199.80 N, and 2921.87 ± 349.67 N for AmannGirrbac, Cercon HT, Cercon XT, and Vita YZ XT, respectively. The mean fracture loads for the surfaces with the greatest number of cracks (excluding the occlusal surfaces) were on the lingual surface for AmannGirrbach and Cercon HT, on the distal and mesial for Cercon XT, and on the buccal for Vita YZ XT. We found that the AmannGirrbach had the most overall cracks. Cercon XT had the greatest number of occlusal cracks and appeared to be the most shattered. Cercon HT had the least number of cracks. In conclusion, Cercon HT presented the best strength properties, the highest fracture load, and no visible cracks. AmannGirrbach presented the lowest strength properties.

read more

Citations
More filters
Journal ArticleDOI

PEEK in Fixed Dental Prostheses: Application and Adhesion Improvement

TL;DR: Polyetheretherketone (PEEK) has been widely applied in fixed dental prostheses, comprising crowns, fixed partial dentures, and post-and-core, and it is nonmutagenic, noncytotoxic, and nonallergenic.
Journal ArticleDOI

Effect of Speed Sintering on Low Temperature Degradation and Biaxial Flexural Strength of 5Y-TZP Zirconia

TL;DR: In this paper , the surface structure, phase determination, translucency, and flexural strength of 5Y-TZP Zirconia (Katana STML Block and Disc) was evaluated with and without low-temperature degradation (LTD).
Journal ArticleDOI

Comparison of Regular and Speed Sintering on Low-Temperature Degradation and Fatigue Resistance of Translucent Zirconia Crowns for Implants: An In Vitro Study

TL;DR: In this paper , the surface structure, cracks, and load-bearing capacity in zirconia screw-retained implant crowns between regular sintering (RS) and speed sinterings (SS) protocol with and without cyclic loading (fatigue).
Journal ArticleDOI

Bending Fracture of Different Zirconia-Based Bioceramics for Dental Applications: A Comparative Study.

TL;DR: In this paper, three-unit full zirconia fixed prosthetic restorations obtained by CAD/CAM technology were tested by bending trials and the results obtained after performing the bending tests showed that a zirconsia material with fewer structural defects and an increased percentage of grain size area under 0.5 µm2, ranging from ~44% in the upper area to ~74% in lower area, exhibited enhanced mechanical behavior.
References
More filters
Journal ArticleDOI

A comparison of the microstructure and properties of the IPS Empress®2 and the IPS Empress® glass‐ceramics

TL;DR: The authors concluded that IPS Empress 2 can be used to fabricate 3-unit bridges up to the second premolar and fulfill the dental standards.
Journal ArticleDOI

Performance of Dental Ceramics Challenges for Improvements

TL;DR: Clinical, experimental, and analytic results reported in the recent literature are summarized to address how this new information adds insight into predictive test procedures and reveals challenges for future improvements.
Journal ArticleDOI

Zirconia based dental ceramics: structure, mechanical properties, biocompatibility and applications.

TL;DR: This systematic review covers the results of past as well as recent scientific studies on the properties of zirconia based ceramics such as their specific compositions, microstructures, mechanical strength, biocompatibility and other applications in dentistry.
Journal ArticleDOI

Phase transitions in zirconium dioxide and related materials for high performance engineering ceramics

TL;DR: In this article, phase transition and transformation toughening in ZrO2 are reviewed with the purpose to understand its effects in some composites and glass systems, taking into account the transformation toughness mechanism that operates in their microstructure.
Journal ArticleDOI

Fracture resistance of monolithic zirconia molar crowns with reduced thickness

TL;DR: It is suggested that monolithic zirconia crown with chamfer width of 0.5 mm and occlusal thickness of 0,5 mm can be used in the molar region in terms of fracture resistance.