scispace - formally typeset
Journal ArticleDOI

Numerical analysis of hydrogen transport near a blunting crack tip

TLDR
In this paper, Oriani's equilibrium theory is used to relate the hydrogen in traps (micro-structural defects) to concentration in normal interstitial lattice sites (NILS), and the resulting non-linear transient hydrogen diffusion equations are integrated using a modified backward Euler method.
Abstract
T he hydrogen transport problem is studied in conjunction with large deformation elastic—plastic behavior of a material. Oriani's equilibrium theory is used to relate the hydrogen in traps (micro-structural defects) to concentration in normal interstitial lattice sites (NILS). The resulting non-linear transient hydrogen diffusion equations are integrated using a modified backward Euler method. Coupled diffusion and plastic straining is analysed with this numerical procedure in the area around a blunting crack tip. A uniform NILS concentration as dictated by Sievert's law at the pressure and temperature of interest is used as initial condition throughout the body. The crack is initially blunted by plane strain mode I (tensile) loading. The finite element results show that hydrogen residing at NILS is generally very small in comparison with the population that develops in trapping sites near the crack surface. That is, lattice diffusion delivers the hydrogen but it is predominantly the trapping that determines its distribution at temperatures of interest. The predominance of trapped hydrogen over lattice concentration prevails even in the case when hydrogen migrates under steady state conditions. Hence, the hydrostatic stress effect is less important than traps created by plastic straining as far as the creation of high total hydrogen concentration is concerned. The trapping site locations and the temperature determine the amounts and locations of high hydrogen concentrations. Consequently, ahead of a blunting crack tip, the total hydrogen concentration and plastic strain diminish with distance from the crack tip whereas the hydrostatic stress rises. This would seem to have significant consequences for fractures induced by the presence of hydrogen.

read more

Citations
More filters
Journal ArticleDOI

Effects of External Hydrogen on Hydrogen Transportation and Distribution Around the Fatigue Crack Tip in Type 304 Stainless Steel

TL;DR: In this article, the effects of external hydrogen on hydrogen transportation and distribution around the fatigue crack tip in type 304 stainless steel were investigated by using hydrogen microprint technique (HMT) and thermal desorption spectrometry.
Journal Article

Microstructural characterization of hydrogen induced cracking in TRIP steels by EBSD

TL;DR: In this paper, the authors evaluated hydrogen induced cracking in a high strength TRIP steel with a complex multiphase microstructure, containing ferrite, bainite, retained austenite, and some martensite.
Journal ArticleDOI

The dependence of fatigue crack growth on hydrogen in warm-rolled 316 austenitic stainless steel

TL;DR: In this paper, the authors investigated the fatigue crack growth rate of AISI 316 austenitic stainless steel by controlling rolling strain and temperature in argon and hydrogen gas atmospheres and found that deformation twins and dislocations became more uniform with the increase in rolling temperature, inhibiting the formation of dynamic α′ martensite during the crack propagation.
Dissertation

Etude des mécanismes de corrosion sous contrainte des aciers inoxydables supermartensitiques en milieu H2S

Martin Monnot
TL;DR: In this paper, the authors present an approach to understandment du mecanisme de corrosion sous contrainte comportant de two etapes : the resistance du film passif and le piegeage de l'hydrogene par l'austenite residuelle.
References
More filters
Book

The finite element method

TL;DR: In this article, the methodes are numeriques and the fonction de forme reference record created on 2005-11-18, modified on 2016-08-08.
Journal ArticleDOI

A Path Independent Integral and the Approximate Analysis of Strain Concentration by Notches and Cracks

TL;DR: In this paper, an integral is exhibited which has the same value for all paths surrounding a class of notches in two-dimensional deformation fields of linear or non-linear elastic materials.
Journal ArticleDOI

Effects of hydrogen on the properties of iron and steel

TL;DR: In this paper, the effects of hydrogen on the physical and mechanical properties of iron and steel are reviewed and a new mechanism for the cold work peak for hydrogen in iron is considered.
Journal ArticleDOI

The diffusion and trapping of hydrogen in steel

TL;DR: In this paper, the mobility of dissolved hydrogen in an iron lattice having a population of extraordinary, or trapping, sites for hydrogen is analyzed under the assumption of local equilibrium between the mobile and the trapped populations.
Book

Hydrogen in metals

Related Papers (5)