Open AccessBook
Practical surface analysis: By auger and x-ray photoelectron spectroscopy
David Briggs,M. P. Seah +1 more
About:
The article was published on 1983-01-01 and is currently open access. It has received 4689 citations till now. The article focuses on the topics: Auger electron spectroscopy & X-ray photoelectron spectroscopy.read more
Citations
More filters
Journal ArticleDOI
Gold nanoparticles stabilized with aromatic thiols: Interaction at the molecule-metal interface and ligand arrangement in the molecular shell investigated by SR-XPS and NEXAFS
Chiara Battocchio,Francesco Porcaro,Subhrangsu Mukherjee,Elena Magnano,Silvia Nappini,Ilaria Fratoddi,Maurizio Quintiliani,Maria Vittoria Russo,Giovanni Polzonetti +8 more
TL;DR: In this article, small gold nanoparticles capped with 4-trimethylsilylethynyl-1-acetylthiobenzene (SEB) were prepared with spherical shape and different mean sizes (5-8 nm).
Journal ArticleDOI
Electrical properties and acetone-sensing characteristics of LaNi1−xTixO3 perovskite system prepared by amorphous citrate decomposition
TL;DR: In this paper, a perovskite type oxides LaNi 1− x Ti x O 3 (x ǫ = 0.0-1.0) were prepared by thermal decomposition of amorphous citrate precursors followed by annealing at 700-1000°C in ambient air.
Journal ArticleDOI
Deposition of polymethyl methacrylate on polypropylene substrates using an atmospheric pressure dielectric barrier discharge
N. De Geyter,Rino Morent,S. Van Vlierberghe,Peter Dubruel,Ch. Leys,Léon Gengembre,Etienne Schacht,Edmond Payen +7 more
TL;DR: In this article, an atmospheric pressure glow-like dielectric barrier discharge in helium with small admixtures of methyl methacrylate (MMA) is used for the deposition of thin PMMA films.
Journal ArticleDOI
Surface modification and characterization of carbon black with oxygen plasma
TL;DR: The surface of carbon black was modified with an oxygen plasma treatment and the initial increase and following reduction of carbon-black weight due to the treatment were observed as the treatment time increased as mentioned in this paper.
Journal ArticleDOI
Nanoscale characterisation of thickness and properties of interphase in polymer matrix composites
Jang Kyo Kim,Alma Hodzic +1 more
TL;DR: In this article, the properties and effective thickness of the interphase formed between fibres and polymer matrices are discussed to portray molecular interactions comprising the inter-phase layers in silane-treated glass-fibre composites.