Journal ArticleDOI
Surface chemistry of atomic layer deposition: A case study for the trimethylaluminum/water process
Reads0
Chats0
TLDR
In this paper, the surface chemistry of the trimethylaluminum/water ALD process is reviewed, with an aim to combine the information obtained in different types of investigations, such as growth experiments on flat substrates and reaction chemistry investigation on high-surface-area materials.Abstract:
Atomic layer deposition(ALD), a chemical vapor deposition technique based on sequential self-terminating gas–solid reactions, has for about four decades been applied for manufacturing conformal inorganic material layers with thickness down to the nanometer range. Despite the numerous successful applications of material growth by ALD, many physicochemical processes that control ALD growth are not yet sufficiently understood. To increase understanding of ALD processes, overviews are needed not only of the existing ALD processes and their applications, but also of the knowledge of the surface chemistry of specific ALD processes. This work aims to start the overviews on specific ALD processes by reviewing the experimental information available on the surface chemistry of the trimethylaluminum/water process. This process is generally known as a rather ideal ALD process, and plenty of information is available on its surface chemistry. This in-depth summary of the surface chemistry of one representative ALD process aims also to provide a view on the current status of understanding the surface chemistry of ALD, in general. The review starts by describing the basic characteristics of ALD, discussing the history of ALD—including the question who made the first ALD experiments—and giving an overview of the two-reactant ALD processes investigated to date. Second, the basic concepts related to the surface chemistry of ALD are described from a generic viewpoint applicable to all ALD processes based on compound reactants. This description includes physicochemical requirements for self-terminating reactions,reaction kinetics, typical chemisorption mechanisms, factors causing saturation, reasons for growth of less than a monolayer per cycle, effect of the temperature and number of cycles on the growth per cycle (GPC), and the growth mode. A comparison is made of three models available for estimating the sterically allowed value of GPC in ALD. Third, the experimental information on the surface chemistry in the trimethylaluminum/water ALD process are reviewed using the concepts developed in the second part of this review. The results are reviewed critically, with an aim to combine the information obtained in different types of investigations, such as growth experiments on flat substrates and reaction chemistry investigation on high-surface-area materials. Although the surface chemistry of the trimethylaluminum/water ALD process is rather well understood, systematic investigations of the reaction kinetics and the growth mode on different substrates are still missing. The last part of the review is devoted to discussing issues which may hamper surface chemistry investigations of ALD, such as problematic historical assumptions, nonstandard terminology, and the effect of experimental conditions on the surface chemistry of ALD. I hope that this review can help the newcomer get acquainted with the exciting and challenging field of surface chemistry of ALD and can serve as a useful guide for the specialist towards the fifth decade of ALD research.read more
Citations
More filters
Journal ArticleDOI
Spatial Atmospheric Atomic Layer Deposition of AlxZn1–xO
TL;DR: The unique combination of the fine tuning of the composition, morphology, and electrical properties of the films with high deposition rates paves the way for spatial ALD as an emerging disruptive technique for the growth of multicomponent oxides over large areas.
Journal ArticleDOI
Graphene functionalization and seeding for dielectric deposition and device integration
TL;DR: Graphene has recently attracted wide-spread attention because of its unique transport and physical properties that are appealing for a wide range of electronic applications, including next generation THz applications.
Journal ArticleDOI
Process-property relationship in high-: K ALD SrTiO3 and BaTiO3: A review
Joon Hyung Shim,Joon Hyung Shim,Hyeju Choi,Yongmin Kim,Jan Torgersen,Jan Torgersen,J. An,M. H. Lee,Fritz B. Prinz +8 more
TL;DR: In this paper, the authors present work on barium and strontium titanate (BTO and STO) ultrathin films for high-k applications and present ALD process strategies developed and optimized to achieve both desired composition and phase, yielding high dielectric constants and low leakage currents.
Journal ArticleDOI
Hot-wire-assisted atomic layer deposition of a high quality cobalt film using cobaltocene: Elementary reaction analysis on NHx radical formation
TL;DR: In this article, a hot-wire-assisted atomic layer deposition (HW-ALD) has been identified as a successful method to form high quality metallic films using metallocene and NH3.
Journal ArticleDOI
Antibacterial and barrier properties of oriented polymer films with ZnO thin films applied with atomic layer deposition at low temperatures
Mika Vähä-Nissi,Marja Pitkänen,Erkki Salo,Eija Kenttä,Anne Tanskanen,Timo Sajavaara,Matti Putkonen,Jenni Sievänen,Asko Sneck,Marjaana Rättö,Maarit Karppinen,Ali Harlin +11 more
TL;DR: In this paper, the properties of zinc oxide thin films compared to those of aluminum oxide were studied and shown to be quite close to those obtained earlier with ALD Al 2 O 3 of similar apparent thickness on similar polymer films.
References
More filters
Journal ArticleDOI
High-κ gate dielectrics: Current status and materials properties considerations
TL;DR: In this paper, a review of the literature in the area of alternate gate dielectrics is given, based on reported results and fundamental considerations, the pseudobinary materials systems offer large flexibility and show the most promise toward success.
Book
Elements of Chemical Reaction Engineering
TL;DR: In this paper, the authors present an approach to scale-up of a continuous-flow-reactor with a CSTR design and demonstrate the performance of the CSTRs.
Book
Basic Inorganic Chemistry
TL;DR: The Periodic Table and the Chemistry of the Elements as discussed by the authors are the main sources of information about the transition elements of the periodic table and their relationships with the transition metal complexes with TT-Acceptor (TT-Acid) ligands.
Journal ArticleDOI
Catalytic Aluminas: Surface Models and Characterization of Surface Sites
Helmut Knözinger,Paul Ratnasamy +1 more
TL;DR: Aluminas have been used extensively as adsorbenu and active catalysrs and catalyst supponsm the pas as discussed by the authors, and they are used as catalysts for the larter process LS also caralyzed by molybdena-alumina.
Journal ArticleDOI
High dielectric constant oxides
TL;DR: In this article, the choice of oxides, their structural and metallurgical behaviour, atomic diffusion, their deposition, interface structure and reactions, their electronic structure, bonding, band offsets, mobility degradation, flat band voltage shifts and electronic defects are discussed.