Surface chemistry of atomic layer deposition: A case study for the trimethylaluminum/water process
Reads0
Chats0
TLDR
In this paper, the surface chemistry of the trimethylaluminum/water ALD process is reviewed, with an aim to combine the information obtained in different types of investigations, such as growth experiments on flat substrates and reaction chemistry investigation on high-surface-area materials.Abstract:
Atomic layer deposition(ALD), a chemical vapor deposition technique based on sequential self-terminating gas–solid reactions, has for about four decades been applied for manufacturing conformal inorganic material layers with thickness down to the nanometer range. Despite the numerous successful applications of material growth by ALD, many physicochemical processes that control ALD growth are not yet sufficiently understood. To increase understanding of ALD processes, overviews are needed not only of the existing ALD processes and their applications, but also of the knowledge of the surface chemistry of specific ALD processes. This work aims to start the overviews on specific ALD processes by reviewing the experimental information available on the surface chemistry of the trimethylaluminum/water process. This process is generally known as a rather ideal ALD process, and plenty of information is available on its surface chemistry. This in-depth summary of the surface chemistry of one representative ALD process aims also to provide a view on the current status of understanding the surface chemistry of ALD, in general. The review starts by describing the basic characteristics of ALD, discussing the history of ALD—including the question who made the first ALD experiments—and giving an overview of the two-reactant ALD processes investigated to date. Second, the basic concepts related to the surface chemistry of ALD are described from a generic viewpoint applicable to all ALD processes based on compound reactants. This description includes physicochemical requirements for self-terminating reactions,reaction kinetics, typical chemisorption mechanisms, factors causing saturation, reasons for growth of less than a monolayer per cycle, effect of the temperature and number of cycles on the growth per cycle (GPC), and the growth mode. A comparison is made of three models available for estimating the sterically allowed value of GPC in ALD. Third, the experimental information on the surface chemistry in the trimethylaluminum/water ALD process are reviewed using the concepts developed in the second part of this review. The results are reviewed critically, with an aim to combine the information obtained in different types of investigations, such as growth experiments on flat substrates and reaction chemistry investigation on high-surface-area materials. Although the surface chemistry of the trimethylaluminum/water ALD process is rather well understood, systematic investigations of the reaction kinetics and the growth mode on different substrates are still missing. The last part of the review is devoted to discussing issues which may hamper surface chemistry investigations of ALD, such as problematic historical assumptions, nonstandard terminology, and the effect of experimental conditions on the surface chemistry of ALD. I hope that this review can help the newcomer get acquainted with the exciting and challenging field of surface chemistry of ALD and can serve as a useful guide for the specialist towards the fifth decade of ALD research.read more
Citations
More filters
Journal ArticleDOI
High dielectric constant gate oxides for metal oxide Si transistors
TL;DR: In this article, a review of the development of high-k gate oxides such as hafnium oxide (HFO) and high-K oxides is presented, with the focus on the work function control in metal gate electrodes.
Journal ArticleDOI
Platinum single-atom and cluster catalysis of the hydrogen evolution reaction
Niancai Cheng,Samantha Stambula,Da Wang,Mohammad Norouzi Banis,Jian Liu,Adam Riese,Biwei Xiao,Ruying Li,Tsun-Kong Sham,Li-Min Liu,Gianluigi A. Botton,Xueliang Sun +11 more
TL;DR: A practical synthesis method to produce isolated single platinum atoms and clusters using the atomic layer deposition technique and indicates that the partially unoccupied density of states of the platinum atoms' 5d orbitals on the nitrogen-doped graphene are responsible for the excellent performance.
Journal ArticleDOI
A brief review of atomic layer deposition: from fundamentals to applications
TL;DR: Atomic layer deposition (ALD) is a vapor phase technique capable of producing thin films of a variety of materials as discussed by the authors, including metal oxides such as Zn1−xSnxOy, ZrO2, Y2O3, and Pt.
Journal ArticleDOI
Crystallinity of inorganic films grown by atomic layer deposition: Overview and general trends
TL;DR: Puurunen et al. as discussed by the authors summarized the two-reactant ALD processes to grow inorganic materials developed to-date, updating the information of an earlier review on ALD.
References
More filters
Journal ArticleDOI
Approaches to understanding MBE growth phenomena
TL;DR: In this paper, a physical model of molecular beam epitaxy (MBE) growth is presented in a consistent form taking into consideration the atomistic nature of crystallization phenomena occurring in this process.
Journal ArticleDOI
Characterization of HfO2/Si(001) interface with high-resolution Rutherford backscattering spectroscopy
Kazuo Nakajima,S. Joumori,Motofumi Suzuki,Kuniko Kimura,Thomas Osipowicz,K. L. Tok,Jia Zhen Zheng,Alex See,B. C. Zhang +8 more
TL;DR: In this paper, the authors used high-resolution Rutherford backscattering spectroscopy (HRBS) and channeling technique to characterize a HfO2 (3nm)/Si(0.0.1) interface prepared by atomic layer chemical vapor deposition.
Journal ArticleDOI
Atomic layer epitaxy of GaAs and GaAsxP1 − x on nominally oriented GaAs(111) substrates with high quality surface and interfaces
TL;DR: In this article, the X-ray rocking curve of the GaAs x P 1 − x GaAs multilayer sample grown on the (111)B substrate showing clear satellite patterns indicates abrupt interfaces that are superior to those of the (100) sample.
Journal ArticleDOI
Effects of Various Oxidizers on the ZrO2 Thin Films Deposited by Atomic Layer Deposition
TL;DR: In this article, the effect of O2 and N2O as an oxidizer of atomic layer deposition (ALD) using Zr tert-butoxide on the characteristics of ZrO2 compared to a conventional reactant, H2O.
Journal ArticleDOI
XPS instrument coupled with ALCVD reactor for investigation of film growth
TL;DR: In this article, a new tool for in situ x-ray photoelectron spectroscopy (XPS) analysis of the atomic layer chemical vapor deposition (ALCVD) process has been developed.