Journal ArticleDOI
Surface chemistry of atomic layer deposition: A case study for the trimethylaluminum/water process
Reads0
Chats0
TLDR
In this paper, the surface chemistry of the trimethylaluminum/water ALD process is reviewed, with an aim to combine the information obtained in different types of investigations, such as growth experiments on flat substrates and reaction chemistry investigation on high-surface-area materials.Abstract:
Atomic layer deposition(ALD), a chemical vapor deposition technique based on sequential self-terminating gas–solid reactions, has for about four decades been applied for manufacturing conformal inorganic material layers with thickness down to the nanometer range. Despite the numerous successful applications of material growth by ALD, many physicochemical processes that control ALD growth are not yet sufficiently understood. To increase understanding of ALD processes, overviews are needed not only of the existing ALD processes and their applications, but also of the knowledge of the surface chemistry of specific ALD processes. This work aims to start the overviews on specific ALD processes by reviewing the experimental information available on the surface chemistry of the trimethylaluminum/water process. This process is generally known as a rather ideal ALD process, and plenty of information is available on its surface chemistry. This in-depth summary of the surface chemistry of one representative ALD process aims also to provide a view on the current status of understanding the surface chemistry of ALD, in general. The review starts by describing the basic characteristics of ALD, discussing the history of ALD—including the question who made the first ALD experiments—and giving an overview of the two-reactant ALD processes investigated to date. Second, the basic concepts related to the surface chemistry of ALD are described from a generic viewpoint applicable to all ALD processes based on compound reactants. This description includes physicochemical requirements for self-terminating reactions,reaction kinetics, typical chemisorption mechanisms, factors causing saturation, reasons for growth of less than a monolayer per cycle, effect of the temperature and number of cycles on the growth per cycle (GPC), and the growth mode. A comparison is made of three models available for estimating the sterically allowed value of GPC in ALD. Third, the experimental information on the surface chemistry in the trimethylaluminum/water ALD process are reviewed using the concepts developed in the second part of this review. The results are reviewed critically, with an aim to combine the information obtained in different types of investigations, such as growth experiments on flat substrates and reaction chemistry investigation on high-surface-area materials. Although the surface chemistry of the trimethylaluminum/water ALD process is rather well understood, systematic investigations of the reaction kinetics and the growth mode on different substrates are still missing. The last part of the review is devoted to discussing issues which may hamper surface chemistry investigations of ALD, such as problematic historical assumptions, nonstandard terminology, and the effect of experimental conditions on the surface chemistry of ALD. I hope that this review can help the newcomer get acquainted with the exciting and challenging field of surface chemistry of ALD and can serve as a useful guide for the specialist towards the fifth decade of ALD research.read more
Citations
More filters
Journal ArticleDOI
Synthesis of two-dimensional MoS2/graphene heterostructure by atomic layer deposition using MoF6 precursor
Youngjun Kim,Daeguen Choi,Whang Je Woo,Jae Bok Lee,Gyeong Hee Ryu,Jun Hyung Lim,Sunhee Lee,Zonghoon Lee,Seongil Im,Jong Hyun Ahn,Woo Hee Kim,Jusang Park,Hyungjun Kim +12 more
TL;DR: In this article, a halide precursor was used for the synthesis of 2D transition metal dichalcogenide (TMD) heterostructures using atomic layer deposition (ALD).
Journal ArticleDOI
A novel approach for fabrication of bismuth-silicon dioxide core-shell structures by atomic layer deposition
Jongmin Lee,Shadyar Farhangfar,Ren Bin Yang,Roland Scholz,Marin Alexe,Ulrich Gösele,Jaeyoung Lee,Kornelius Nielsch +7 more
TL;DR: In this article, Bismuth (Bi) nanowires were grown electrochemically into the pores of anodic aluminium oxide (AAO) templates and showed a highly preferential growth orientation along the (110) direction.
Journal ArticleDOI
Surface passivation of aluminum hydride particles via atomic layer deposition
TL;DR: In this paper, conformal amorphous Al2O3 films were coated around the crystalline α-AlH3 particles, serving as physical barriers to prevent reactions, and the retained hydrogen capacity of passivated particles was four times higher than the untreated sample.
Journal ArticleDOI
Magnetic tunnel junctions with Al2O3 tunnel barriers prepared by atomic layer deposition
Xinfei Liu,Jing Shi +1 more
TL;DR: In this article, the tunneling magnetoresistance in optimized Al2O3-based magnetic tunnel junctions is studied as a function of temperature in comparison with SrTiO3based tunnel devices having the same La0.7Sr0.3MnO3 and Co electrodes.
Journal ArticleDOI
Effect of atomic layer deposition temperature on current conduction in Al2O3 films formed using H2O oxidant
TL;DR: In this paper, the effect of atomic layer deposition (ALD) temperature on current conduction in Al2O3 capacitors is investigated based on the recently proposed space-charge-controlled field emission model.
References
More filters
Journal ArticleDOI
High-κ gate dielectrics: Current status and materials properties considerations
TL;DR: In this paper, a review of the literature in the area of alternate gate dielectrics is given, based on reported results and fundamental considerations, the pseudobinary materials systems offer large flexibility and show the most promise toward success.
Book
Elements of Chemical Reaction Engineering
TL;DR: In this paper, the authors present an approach to scale-up of a continuous-flow-reactor with a CSTR design and demonstrate the performance of the CSTRs.
Book
Basic Inorganic Chemistry
TL;DR: The Periodic Table and the Chemistry of the Elements as discussed by the authors are the main sources of information about the transition elements of the periodic table and their relationships with the transition metal complexes with TT-Acceptor (TT-Acid) ligands.
Journal ArticleDOI
Catalytic Aluminas: Surface Models and Characterization of Surface Sites
Helmut Knözinger,Paul Ratnasamy +1 more
TL;DR: Aluminas have been used extensively as adsorbenu and active catalysrs and catalyst supponsm the pas as discussed by the authors, and they are used as catalysts for the larter process LS also caralyzed by molybdena-alumina.
Journal ArticleDOI
High dielectric constant oxides
TL;DR: In this article, the choice of oxides, their structural and metallurgical behaviour, atomic diffusion, their deposition, interface structure and reactions, their electronic structure, bonding, band offsets, mobility degradation, flat band voltage shifts and electronic defects are discussed.