Journal ArticleDOI
Surface chemistry of atomic layer deposition: A case study for the trimethylaluminum/water process
Reads0
Chats0
TLDR
In this paper, the surface chemistry of the trimethylaluminum/water ALD process is reviewed, with an aim to combine the information obtained in different types of investigations, such as growth experiments on flat substrates and reaction chemistry investigation on high-surface-area materials.Abstract:
Atomic layer deposition(ALD), a chemical vapor deposition technique based on sequential self-terminating gas–solid reactions, has for about four decades been applied for manufacturing conformal inorganic material layers with thickness down to the nanometer range. Despite the numerous successful applications of material growth by ALD, many physicochemical processes that control ALD growth are not yet sufficiently understood. To increase understanding of ALD processes, overviews are needed not only of the existing ALD processes and their applications, but also of the knowledge of the surface chemistry of specific ALD processes. This work aims to start the overviews on specific ALD processes by reviewing the experimental information available on the surface chemistry of the trimethylaluminum/water process. This process is generally known as a rather ideal ALD process, and plenty of information is available on its surface chemistry. This in-depth summary of the surface chemistry of one representative ALD process aims also to provide a view on the current status of understanding the surface chemistry of ALD, in general. The review starts by describing the basic characteristics of ALD, discussing the history of ALD—including the question who made the first ALD experiments—and giving an overview of the two-reactant ALD processes investigated to date. Second, the basic concepts related to the surface chemistry of ALD are described from a generic viewpoint applicable to all ALD processes based on compound reactants. This description includes physicochemical requirements for self-terminating reactions,reaction kinetics, typical chemisorption mechanisms, factors causing saturation, reasons for growth of less than a monolayer per cycle, effect of the temperature and number of cycles on the growth per cycle (GPC), and the growth mode. A comparison is made of three models available for estimating the sterically allowed value of GPC in ALD. Third, the experimental information on the surface chemistry in the trimethylaluminum/water ALD process are reviewed using the concepts developed in the second part of this review. The results are reviewed critically, with an aim to combine the information obtained in different types of investigations, such as growth experiments on flat substrates and reaction chemistry investigation on high-surface-area materials. Although the surface chemistry of the trimethylaluminum/water ALD process is rather well understood, systematic investigations of the reaction kinetics and the growth mode on different substrates are still missing. The last part of the review is devoted to discussing issues which may hamper surface chemistry investigations of ALD, such as problematic historical assumptions, nonstandard terminology, and the effect of experimental conditions on the surface chemistry of ALD. I hope that this review can help the newcomer get acquainted with the exciting and challenging field of surface chemistry of ALD and can serve as a useful guide for the specialist towards the fifth decade of ALD research.read more
Citations
More filters
Journal ArticleDOI
High dielectric constant gate oxides for metal oxide Si transistors
TL;DR: In this article, a review of the development of high-k gate oxides such as hafnium oxide (HFO) and high-K oxides is presented, with the focus on the work function control in metal gate electrodes.
Journal ArticleDOI
Platinum single-atom and cluster catalysis of the hydrogen evolution reaction
Niancai Cheng,Samantha Stambula,Da Wang,Mohammad Norouzi Banis,Jian Liu,Adam Riese,Biwei Xiao,Ruying Li,Tsun-Kong Sham,Li-Min Liu,Gianluigi A. Botton,Xueliang Sun +11 more
TL;DR: A practical synthesis method to produce isolated single platinum atoms and clusters using the atomic layer deposition technique and indicates that the partially unoccupied density of states of the platinum atoms' 5d orbitals on the nitrogen-doped graphene are responsible for the excellent performance.
Journal ArticleDOI
A brief review of atomic layer deposition: from fundamentals to applications
TL;DR: Atomic layer deposition (ALD) is a vapor phase technique capable of producing thin films of a variety of materials as discussed by the authors, including metal oxides such as Zn1−xSnxOy, ZrO2, Y2O3, and Pt.
Journal ArticleDOI
Crystallinity of inorganic films grown by atomic layer deposition: Overview and general trends
TL;DR: Puurunen et al. as discussed by the authors summarized the two-reactant ALD processes to grow inorganic materials developed to-date, updating the information of an earlier review on ALD.
References
More filters
Journal ArticleDOI
GaAs/AlGaAs quantum well lasers with active regions grown by atomic layer epitaxy
TL;DR: In this article, the use of ALE to grow high-quality GaAs/AlGaAs quantum wells and the first successful demonstration of an injection laser with a quantum well active region grown by ALE are described.
Journal ArticleDOI
Comparison between atomic-layer-deposited HfO2 films using O3 or H2O oxidant and Hf[N(CH3)2]4 precursor
Moonju Cho,Doo Seok Jeong,Jaehoo Park,Hong-bae Park,Suk Woo Lee,Tae Joo Park,Cheol Seong Hwang,Gi Hoon Jang,Jaehack Jeong +8 more
TL;DR: In this article, the dielectric properties of HfO2 thin films, which were deposited on Si wafers by an atomic layer deposition (ALD) technique at a wafer temperature of 300 °C using a N-containing, tetrakis dimethylamido hafnium precursor (Hf[N(CH3)2]4), were highly improved by adopting O3 as the oxidant during the ALD instead of H2O.
Journal ArticleDOI
Characterization of titanium dioxide atomic layer growth from titanium ethoxide and water
TL;DR: In this paper, the atomic layer growth of titanium dioxide from titanium ethoxide and water was studied, and it was shown that the deposition rate reached 0.06 nm per cycle at optimized precursor doses and the refractive index reached 2.5 at the wavelength 580 nm.
Journal ArticleDOI
Studies on polycrystalline ZnS thin films grown by atomic layer deposition for electroluminescent applications
Yong Shin Kim,Sun Jin Yun +1 more
TL;DR: In this paper, polycrystalline ZnS thin films were grown by the atomic layer deposition (ALD) using the precursors of diethyl zinc and hydrogen sulfide in the substrate temperature range of 250-400°C.
Journal ArticleDOI
Fabrication of titanium oxide thin films by controlled growth with sequential surface chemical reactions
TL;DR: In this article, a novel vapor combination of tetrachlorotitanium (TiCl4) and hydrogen peroxide (H2O2) was used to control growth of titanium oxide films by sequential surface chemical reactions.